Slane, J., Vivanco, J. F., Squire, M., & Ploeg, H. L. (2017). Characterization of the quasi-static and viscoelastic properties of orthopaedic bone cement at the macro and nanoscale. J. Biomed. Mater. Res. Part B, 105(6), 1461–1468.
toggle visibility
Norambuena-Contreras, J., Gonzalez-Torre, I., Vivanco, J. F., & Gacitua, W. (2016). Nanomechanical properties of polymeric fibres used in geosynthetics. Polym. Test, 54, 67–77.
toggle visibility
Slane, J., Vivanco, J., Ebenstein, D., Squire, M., & Ploeg, H. L. (2014). Multiscale characterization of acrylic bone cement modified with functionalized mesoporous silica nanoparticles. J. Mech. Behav. Biomed. Mater., 37, 141–152.
toggle visibility
Vivanco, J., Jakes, J. E., Slane, J., & Ploeg, H. L. (2014). Accounting for structural compliance in nanoindentation measurements of bioceramic bone scaffolds. Ceram. Int., 40(8), 12485–12492.