Author Araya-Letelier, G.; Antico, F.C.; Burbano-Garcia, C.; Concha-Riedeld, J.; Norambuena-Contreras, J.; Concha, J.; Saavedra Flores, E.I. doi  openurl
  Title Experimental evaluation of adobe mixtures reinforced with jute fibers Type
  Year 2021 Publication Construction and Building Materials Abbreviated Journal Constr. Build. Mater.  
  Volume 276 Issue 2021 Pages 122127  
  Keywords Jute fibers; Fiber-reinforced composites; Thermal conductivity; Mechanical characterization; Damage and durability assessment  
  Abstract Due to their sustainability as well as physical and mechanical performance, different natural fibers, both vegetal and animal fibers, have been successfully used in adobe mixtures (AMs) to enhance properties such as cracking control, flexural toughness and water erosion resistance, among others. However, the use of jute fibers (JFs), one of the most largely produced vegetal fiber worldwide, has not been extensively studied on AMs. Consequently, this study evaluates the effects of the incorporation of varying dosages (0.5 and 2.0 wt%) and lengths (7, 15, and 30 mm) of JFs on the physical/thermal/mechanical/fracture and durability performance of AMs, a specific type of earth-based construction material widely used globally. Experimental results showed that the incorporation of 2.0 wt% dosages of JFs increased the capillary water absorption of AMs, which might affect AM durability. The latter result could be explained by the additional porosity generated by the spaces left between the JFs and the matrix of adobe, as well as the inherent water absorption of the JFs. The incorporation of JFs significantly improved the behavior of AMs in terms of thermal conductivity, drying shrinkage cracking control, flexural toughness and water erosion performance, without affecting their compressive and flexural strength. For example, flexural toughness indices were increased by 297% and crack density ratio as well as water erosion depth values were reduced by 93% and 62%, respectively, when 2.0 wt%-15 mm length JFs were incorporated into AM. Since the latter combination of JF dosage and length provided the overall best results among AMs, it is recommended by this study as JF-reinforcement scheme for AMs for construction applications such as adobe masonry and earth plasters.  
  Address  
  Corporate Author Thesis  
  Publisher Place of Publication Editor  
  Language Summary Language Original Title  
  Series Editor Series Title Abbreviated Series Title  
  Series Volume Series Issue Edition  
  ISSN 0950-0618 ISBN Medium  
  Area Expedition (up) Conference  
  Notes Approved  
  Call Number UAI @ alexi.delcanto @ Serial 1315  